Material Notes:
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Melt Flow 1.0 - 4.0 g/10 min
1.0 - 4.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
10 sec; ASTM D-2240
Tensile Strength, Ultimate >= 3.45 MPa
>= 500 psi
ASTM D412
Elongation at Break >= 300 %
>= 300 %
ASTM D412
Tear Strength 27.15 kN/m
154.9 pli
ASTM D624