Material Notes:
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Melt Flow 0.85 g/10 min
0.85 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
10 sec; ASTM D-2240
Tensile Strength, Ultimate 5.30 MPa
769 psi
ASTM D638
Elongation at Break 950 %
950 %
ASTM D638
100% Modulus 0.00190 GPa
0.276 ksi
ASTM D412
Tear Strength 29.8 kN/m
170 pli
ASTM D624
Compression Set 56 %

@Temperature 100 °C
56 %

@Temperature 212 °F
for 22 hours at 100°C; ASTM 395