Material Notes:
Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 43
43
10 sec; ASTM D-2240
Tensile Strength, Ultimate >= 5.17 MPa
>= 750 psi
ASTM D412
Elongation at Break >= 760 %
>= 760 %
ASTM D412
Tear Strength >= 19.26 kN/m
>= 109.9 pli
ASTM D624
Compression Set 17 %
17 %
for 70 hours at 23°C; ASTM 395 (Method B)