Multibase Multi-Flex® TPE A 5002 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 5002 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.075 g/cc
0.03884 lb/in³
ASTM D792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Melt Flow 2.0 - 5.0 g/10 min
2.0 - 5.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
10 sec; ASTM D-2240
Tensile Strength, Ultimate >= 3.62 MPa
>= 525 psi
ASTM D412
Elongation at Break >= 600 %
>= 600 %
ASTM D412
Tear Strength >= 20.14 kN/m
>= 114.9 pli
ASTM D624