Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPE 6568 C 1 NATURAL

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE 6568 C 1 NATURAL.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product was designed for 2 shot airbag covers with lower tensile strength than currently in use. The moisture content is 1%. The fogging test value is 70% according to ASTM GM 9305P. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 25 g/10 min
25 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 46
46
10 sec; ASTM D-2240
Tensile Strength, Ultimate 3.00 MPa
435 psi
ASTM D412
Elongation at Break >= 700 %
>= 700 %
ASTM D412
Tear Strength 17.5 kN/m
99.9 pli
ASTM D624