Multibase Multi-Flex® G 7827 Black TPE Styrene Ethylene Butylene Styrene Block Copolymer

Category Polymer , Thermoplastic
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® G 7827 Black TPE Styrene Ethylene Butylene Styrene Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Methods:Injection Molding Uses: Automotive ApplicationsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM 792
Melt Flow 60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
10 seconds; ASTM D2240
Tensile Strength, Yield 10.3 MPa
1500 psi
ASTM D638
Elongation at Break 550 %
550 %
ASTM D638
Flexural Modulus 0.138 GPa
20.0 ksi
ASTM D790
Tear Strength 61.4 kN/m
350 pli
ASTM D624
Thermal Properties Metric English Comments
Flame Spread 22.9 mm/min
0.902 in/min
FM VSS-302