Multibase Multi-Flex® G 7150 TPE Styrene Ethylene Butylene Styrene Block Copolymer

Category Polymer , Thermoplastic
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® G 7150 TPE Styrene Ethylene Butylene Styrene Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.85 g/cc
1.85 g/cc
ASTM 792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
10 seconds; ASTM D2240
Tensile Strength, Yield 4.83 MPa
700 psi
ASTM D638
4.14 MPa

@Strain 300 %
600 psi

@Strain 300 %
ASTM D412
Elongation at Break 450 %
450 %
ASTM D638
Tear Strength 29.8 kN/m
170 pli
ASTM D624