Material Notes:
Features: Chemical Resistance, Good PaintableOzone Resistant General PurposeDensity, LowTear Strength, GoodUV Resistance, Good Forms:PelletsProcessing Method:Blow Molding Uses: Automotive ApplicationsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.882 g/cc
0.882 g/cc
ASTM 792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
10 seconds; ASTM D2240
Tensile Strength, Yield 29.0 MPa
4200 psi
Elastic; ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Izod Impact, Notched 3.74 J/cm
7.00 ft-lb/in
ASTM D256
Tear Strength 87.7 kN/m
500 pli
ASTM D624