Material Notes:
Forms: PelletsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.922 g/cc
0.922 g/cc
ASTM 792
Melt Flow 26 g/10 min

@Load 2.16 kg,
Temperature 230 °C
26 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
10 seconds; ASTM D2240
Tensile Strength, Ultimate 13.79 MPa
2000 psi
Elongation at Break 120 %
120 %
Elastic; ASTM D412
Flexural Modulus 0.524 GPa
76.0 ksi
Method I (3 point load), Procedure B); ASTM D790
Tear Strength 87.7 kN/m
500 pli
ASTM D624