Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® D 5304 Black TPO Thermoplastic Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyolefin
Manufacturer Multibase
Trade Name Multi-Flex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® D 5304 Black TPO Thermoplastic Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.912 g/cc
0.912 g/cc
ASTM 792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 47
47
10 seconds; ASTM D2240
Tensile Strength, Yield 18.8 MPa
2720 psi
Elastic; ASTM D412
Elongation at Break 610 %
610 %
Elastic; ASTM D412
Flexural Modulus 0.329 GPa
47.7 ksi
ASTM D790
Tear Strength 103 kN/m
590 pli
ASTM D624
Processing Properties Metric English Comments
Rear Barrel Temperature 240 °C
464 °F
Middle Barrel Temperature 240 °C
464 °F
Front Barrel Temperature 250 °C
482 °F
Nozzle Temperature 245 °C
473 °F
Mold Temperature 30.0 - 40.0 °C
86.0 - 104 °F