Material Notes:
Features: Chemical Resistance, Good Thermal Stability, GoodOzone Resistant Noise Damping Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.92 g/cc
1.92 g/cc
ASTM 792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 93
93
10 seconds; ASTM D2240
Tensile Strength, Yield 5.52 MPa
800 psi
Elastic; ASTM D638
Elongation at Break 320 %
320 %
ASTM D638
Flexural Modulus 0.310 GPa
45.0 ksi
ASTM D790
Tear Strength 35.1 kN/m
200 pli
ASTM D624