Material Notes:
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM 792
Melt Flow 19.2 g/10 min

@Load 2.16 kg,
Temperature 230 °C
19.2 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 93
93
10 seconds; ASTM D2240
Tensile Strength, Yield 4.97 MPa
721 psi
Elastic; ASTM D412
Elongation at Break 180 %
180 %
Elastic; ASTM D412
Flexural Modulus 0.293 GPa
42.5 ksi
1% Secant; ASTM D790
Tear Strength 35.1 kN/m
200 pli
ASTM D624