Material Notes:
Features: Chemical Resistance, Good Heat StabilizedOzone ResistantGeneral Purpose Friction, Low Processability, Good Forms:PelletsProcessing Method:ExtrusionInjection Molding Uses: Automotive ApplicationsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM 792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
10 seconds; ASTM D2240
Tensile Strength, Yield 2.72 MPa
395 psi
at 100% secant; ASTM D638
12.8 MPa
1850 psi
Elastic; ASTM D638
Elongation at Break 730 %
730 %
ASTM D638
Tear Strength 43.8 kN/m
250 pli
ASTM D624
Compression Set 28 %
28 %
73°F, 70 hours; ASTM D395
76 %
76 %
158°F, 70 hours; ASTM D395