Multibase Multi-Flex® A 7204 LC TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® A 7204 LC TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good Processability, GoodForms:PelletsProcessing Method:Extrusion Uses: GasketsTubingInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM 792
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
10 seconds; ASTM D2240
Tensile Strength, Yield 2.76 MPa
400 psi
at 100%; ASTM D412
8.96 MPa
1300 psi
Elastic; ASTM D412
Elongation at Break 550 %
550 %
Elastic; ASTM D412
Tear Strength 33.3 kN/m
190 pli
ASTM D624
Compression Set 23 %
23 %
73°F, 70 hours; ASTM D395
45 %
45 %
158°F, 70 hours; ASTM D395
Processing Properties Metric English Comments
Die Temperature 204 °C
400 °F
Melt Temperature 191 - 204 °C
375 - 400 °F