Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® A 6502 MR Natural TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® A 6502 MR Natural TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.932 g/cc
0.932 g/cc
ASTM 792
Melt Flow 1.7 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.7 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
10 seconds; ASTM D2240
Tensile Strength at Break 5.10 MPa
740 psi
ASTM D412
Elongation at Break 690 %
690 %
Elastic; ASTM D412
Tear Strength 36.8 kN/m
210 pli
ASTM D624
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved