Material Notes:
Forms: PelletsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM 792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
10 seconds; ASTM D2240
Tensile Strength, Ultimate 5.17 MPa
750 psi
ASTM D638
Elongation at Break 650 %
650 %
ASTM D638
Flexural Modulus 0.0345 GPa
5.00 ksi
ASTM D790
Tear Strength 24.5 kN/m
140 pli
ASTM D624
Compression Set 17 %
17 %
73°F; ASTM D395