Material Notes:
Features: Chemical Resistance, Good Heat StabilizedOzone Resistant Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM 792
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
10 seconds; ASTM D2240
Tensile Strength, Yield 1.72 MPa
250 psi
at 100% secant; ASTM D638
7.58 MPa
1100 psi
Elastic; ASTM D638
Elongation at Break 580 %
580 %
ASTM D638
Tear Strength 26.3 kN/m
150 pli
ASTM D624
Compression Set 16 %
16 %
73°F, 70 hours; ASTM D395
38 %
38 %
158°F, 70 hours; ASTM D395