Material Notes:
Features:Heat Resistance, GoodThermal Stability, GoodForms:PelletsProcessing Method:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM 792
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
10 seconds; ASTM D2240
Tensile Strength, Yield 1.17 MPa
170 psi
at 100% secant; ASTM D412
5.00 MPa
725 psi
Elastic; ASTM D638
Elongation at Break 700 %
700 %
ASTM D638
Tear Strength 21.0 kN/m
120 pli
ASTM D624
Compression Set 15 %
15 %
73°F, 70 hours; ASTM D395
74 %
74 %
158°F, 70 hours; ASTM D395