Material Notes:
Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Blow MoldingExtrusionCoextrusionUses:TubingFurniturePipingInformation provided by Multibase
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Melt Flow 0.60 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.60 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.8 MPa
3300 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Modulus 1.21 GPa
175 ksi
ASTM D790
Izod Impact, Notched 5.87 J/cm
11.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
0.125 in