Multibase Multi-ABS 3845 Medium Impact ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Multibase
Trade Name Multi-ABS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-ABS 3845 Medium Impact ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955-89
Melt Flow 5.0 g/10 min
5.0 g/10 min
(Condition I) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785-95
Tensile Strength, Ultimate 42.7 MPa
6190 psi
ASTM D638-95
Elongation at Break 35 %
35 %
ASTM D638-95
Flexural Modulus 2.62 GPa
380 ksi
RT; ASTM D-790-95
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
injection molded unannealed; ASTM D-648-95
220 °C
428 °F
injection molded annealed; ASTM D-648-95
220 °C
428 °F
compression molded annealed; ASTM D-648-95
Vicat Softening Point 99.0 °C
210 °F
ASTM D1525-95
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
HB

@Thickness 3.17 mm
HB

@Thickness 0.125 in
Optical Properties Metric English Comments
Gloss 85 - 92 %
85 - 92 %
ASTM D2457-90
Users viewing this material also viewed the following: