Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-ABS 3525 Clear

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Multibase
Trade Name Multi-ABS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-ABS 3525 Clear.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792-91
Melt Flow 5.0 g/10 min
5.0 g/10 min
(Condition I) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM D785-95
Tensile Strength, Ultimate 31.0 MPa
4500 psi
ASTM D638-95
Elongation at Break 25 %
25 %
ASTM D638-95
Flexural Strength 69.0 MPa
10000 psi
ASTM D790-95
Flexural Modulus 2.414 GPa
350.1 ksi
RT; ASTM D-790-95
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256-93a
Optical Properties Metric English Comments
Gloss 40 - 70 %
40 - 70 %
ASTM D2457-90
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Copyright © lookpolymers.com All Rights Reserved