Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Melt Flow 6.0 g/10 min
6.0 g/10 min
(Condition G) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785-95
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D638-95
Elongation at Break 30 %
30 %
ASTM D638-95
Flexural Strength 65.5 MPa
9500 psi
ASTM D790-95
Flexural Modulus 2.228 GPa
323.1 ksi
RT; ASTM D-790-95
Izod Impact, Notched 2.14 J/cm
4.01 ft-lb/in
ASTM D256-93a
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 185 °C
365 °F
injection molded unannealed; ASTM D-648-95
203 °C
397 °F
injection molded annealed; ASTM D-648-95
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525-95
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in