Material Notes:
As part of the Mueller Brass Company’s EcoStream™ family of alloys & products, GreenDrop™ C27450 Lead Free Brass is the ideal material solution for manufacturers required to comply with local & national lead free legislation. With the manufacturer in mind, Mueller Brass Company has developed its GreenDrop™ C27450 Lead Free Brass to not only aid in lead free compliance, but to optimize manufacturing efficiencies through productivity & complete recyclability. No Silicon • No Bismuth • No Segregation Because no detrimental additives or potential contaminants like silicon or bismuth are added, GreenDrop™ C27450 Lead Free Brass is completely recyclable with standard brass alloys that are commonly used today. Without having to retrofit existing scrap handling systems, losing precious machine time cleaning out machines for fear of contaminating valuable brass scrap, Mueller Brass Company’s GreenDrop™ can easily be integrated into production & can readily co-exist with conventional alloys like C36000, C34500, C37700 etc. Advantanges:Good machinabilityExcellent forgeabilityExcellent brazing and platingExcellent ability to Thread RollDezincification ResistantApplications:Potable water components, fixtures and applicationsPEX plumbing applications and systemsForged products requiring lead free and/or dezincification complianceInformation Provided by Mueller Industries Inc.
Mechanical Properties Metric English Comments
Hardness, Rockwell B 55 - 75
55 - 75
Tensile Strength at Break 400 MPa
58000 psi
Tensile Strength, Yield 276 MPa
40000 psi
Elongation at Break 30 %
30 %
Machinability 70 %
70 %
Forgeability 95 %
95 %
Component Elements Properties Metric English Comments
Copper, Cu 60 - 65 %
60 - 65 %
Iron, Fe <= 0.35 %
<= 0.35 %
Lead, Pb <= 0.25 %
<= 0.25 %
Other <= 0.50 %
<= 0.50 %
Zinc, Zn 33.9 - 40 %
33.9 - 40 %
Remainder
Descriptive Properties Value Comments
Brazing Excellent
Cold Working Excellent
Plating Excellent
Soldering Excellent