Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mueller Ecostreamâ„¢ C36300 Copper Zinc Lead Alloy

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer Mueller Industries Inc.
Trade Name Ecostream™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mueller Ecostreamâ„¢ C36300 Copper Zinc Lead Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
As one of the low lead alloys offered in the EcoStream™ family of products, Mueller Brass Company’s C36300 alloy provides a viable alternative to those manufacturers who are manufacturing products and components that require compliance with the recently approved “Reduction of Lead in Drinking Water Act.” The legislation re-defines the term “lead free” to mean “… no more that a weighted average of 0.25% lead when used with respect to the wetted surfaces of pipes, plumbing fittings and fixtures.” No Silicon – No Bismuth – No Segregation Mueller Brass Company’s C36300 alloy provides a lower lead brass alloy option that aids with the compliance strategies of manufacturers who seek an alternative that is not only COMPLIANT, but also COMPETITIVE and COMPATIBLE with standard free cutting and forgings alloys commonly used today. Having significantly less copper than alternative alloys offered by other manufacturers, and not displacing the lead with potentially detrimental additives like bismuth or silicon, C36300 is a competitive solution that affords compliance while maintaining critical aspects of productivity and efficiencies. The turnings, chips and other resulting scrap generated from C36300 is completely compatible with the free cutting (i.e. C36000) and forging alloys (C37700) used industry wide. By virtually eliminating the necessity to segregate, clean out machines, or potentially risk contaminating ‘conventional’ scrap, valuable machine time is further maximized.Advantanges:Excellent machinabilityGood hot forgeabilityExcellent capability for brazing and platingExcellent ability to thread rolledImproved resistance to dezincificationApplications:Screw machine parts and components for potable water products requiring lead free complianceForged parts and components for potable water products requiring lead free complianceInformation Provided by Mueller Industries Inc.
Mechanical Properties Metric English Comments
Hardness, Rockwell B 65

@Diameter 25.4 mm
65

@Diameter 1.00 in
Rod H02
68

@Diameter 12.7 - 25.4 mm
68

@Diameter 0.500 - 1.00 in
Rod H02
Tensile Strength 379 MPa

@Diameter 25.4 mm
55000 psi

@Diameter 1.00 in
Rod H02
414 MPa

@Diameter 12.7 - 25.4 mm
60000 psi

@Diameter 0.500 - 1.00 in
Rod H02
Tensile Strength, Yield 138 MPa

@Diameter 25.4 mm
20000 psi

@Diameter 1.00 in
Rod H02
172 MPa

@Diameter 12.7 - 25.4 mm
25000 psi

@Diameter 0.500 - 1.00 in
Rod H02
Elongation at Break 10 %

@Diameter 12.7 - 25.4 mm
10 %

@Diameter 0.500 - 1.00 in
Rod H02
15 %

@Diameter <=25.4 mm
15 %

@Diameter <=1.00 in
Rod H02
Component Elements Properties Metric English Comments
Copper, Cu 61 - 63 %
61 - 63 %
Iron, Fe <= 0.15 %
<= 0.15 %
Lead, Pb 0.25 - 0.70 %
0.25 - 0.70 %
Phosphorous, P 0.040 - 0.15 %
0.040 - 0.15 %
Zinc, Zn 35.50 - 38.71 %
35.50 - 38.71 %
Remainder
Users viewing this material also viewed the following: