Mueller Alloy 4850 Naval Brass - High Leaded (UNS C48500)

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer Mueller Industries Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mueller Alloy 4850 Naval Brass - High Leaded (UNS C48500).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alloy noted for its machinability and resistance to wear, fatigue, galling and stress corrosion crackingApplications: The alloy is typically used for fastener, valve stems, screw machine products and marine hardware.Information Provided by Mueller Industries Inc.
Mechanical Properties Metric English Comments
Hardness, Rockwell B 82
82
Tensile Strength at Break 517 MPa
75000 psi
Tensile Strength, Yield 365 MPa
53000 psi
Elongation at Break 15 %
15 %
Machinability 70 %
70 %
UNS C36000 = 100%
Component Elements Properties Metric English Comments
Copper, Cu 59 - 62 %
59 - 62 %
Iron, Fe 2.1 %
2.1 %
Lead, Pb 1.3 - 2.2 %
1.3 - 2.2 %
Tin, Sn 0.50 - 1.0 %
0.50 - 1.0 %
Zinc, Zn 32.7 - 37.1 %
32.7 - 37.1 %
Remainder