Material Notes:
Dezincification resistant brass suitable for high speed machining applicationsApplications: The alloy is best suitable where potential corrosion (such as dezincification) may occur. Applications for this alloy include plumber's hardware, valve spindles and fittings.Information Provided by Mueller Industries Inc.
Mechanical Properties Metric English Comments
Hardness, Rockwell B 60
60
Tensile Strength at Break 372 MPa
54000 psi
Tensile Strength, Yield 165 MPa
24000 psi
Elongation at Break 30 %
30 %
Machinability 100 %
100 %
UNS C36000 = 100%
Component Elements Properties Metric English Comments
Arsenic, As 0.020 - 0.25 %
0.020 - 0.25 %
Copper, Cu 59.5 - 64 %
59.5 - 64 %
Lead, Pb 1.5 - 3.5 %
1.5 - 3.5 %
Zinc, Zn 32.25 - 39 %
32.25 - 39 %
Remainder