Mueller Alloy 3450 Leaded Brass (UNS C34500)

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer Mueller Industries Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mueller Alloy 3450 Leaded Brass (UNS C34500).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used for screw machine products requiring some cold formability (i.e. crimping, knurling)Applications: The 3450 is used for screw machine applications requiring the ability to be cold formed either during, or subsequent to, machining. The material can be thread rolled, knurled, bent, flared, swaged or staked. Alloy 3450 exhibits somewhat superior ductility in relation to comparable (i.e. alloy 3530) alloys. Typical applications include valve terms, adapters, couplings, gears, pinions, flare fittings.Information Provided by Mueller Industries Inc.
Mechanical Properties Metric English Comments
Hardness, Rockwell B 66
66
Tensile Strength at Break 372 MPa
54000 psi
Tensile Strength, Yield 234 MPa
34000 psi
Elongation at Break 35 %
35 %
Machinability 90 %
90 %
UNS C36000 = 100%
Component Elements Properties Metric English Comments
Copper, Cu 62 - 65 %
62 - 65 %
Iron, Fe <= 0.15 %
<= 0.15 %
Lead, Pb 1.5 - 2.5 %
1.5 - 2.5 %
Zinc, Zn 32.5 - 36.5 %
32.5 - 36.5 %
Remainder
Processing Properties Metric English Comments
Processing Temperature 260 °C
500 °F
Stress Relieving