Monmouth Rubber & Plastics Superbounce 90 NEO/SBR

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Monmouth Rubber & Plastics
Trade Name Superbounce
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Monmouth Rubber & Plastics Superbounce 90 NEO/SBR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Monmouth Rubber & Plastics Corp.
Physical Properties Metric English Comments
Density >= 0.721 g/cc
>= 0.0260 lb/in³
Water Absorption <= 1.0 %
<= 1.0 %
ASTM D1056
Mechanical Properties Metric English Comments
Hardness, Shore OO 80 - 90
80 - 90
ASTM D2240
Tensile Strength 8.791 MPa
1275 psi
ASTM D2000
Elongation at Break 862 %
862 %
ASTM D2000
Compressive Strength 0.517 - 0.586 MPa
75.0 - 85.0 psi
0.25; ASTM D1056
Tear Strength 42.1 kN/m
240 pli
Die C; ASTM D3575 Suf. G
Compression Set 8.0 %

@Time 86400 sec
8.0 %

@Time 24.0 hour
10 %

@Time 3600 sec
10 %

@Time 1.00 hour
14 %

@Time 60.0 sec
14 %

@Time 0.0167 hour
14 %

@Time 299 sec
14 %

@Time 0.0830 hour
20 %

@Time 5.00 sec
20 %

@Time 0.00139 hour
Descriptive Properties Value Comments
C/D Heat Aging 0.3
7 days @158°F, Change; ASTM D1056
Color Black
Compression Recovery 0.9
5 sec; ASTM D1056
0.93
60 sec; ASTM D1056
0.95
5 mins; ASTM D1056
0.95
60 mins; ASTM D1056
0.96
24 hrs; ASTM D1056
Fluid Immersion 0.2
Oil, Ref Fuel B, ASTM D1056
G Max Rating Vertical energy imput 163 G's
8.8/FT Second; ASMT F1292-99
235 G's
10.5/FT Second; ASMT F1292-99
86 G's
6.6/FT Second; ASMT F1292-99