Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Monmouth Rubber & Plastics Durafoam™ P192HD EPDM

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Monmouth Rubber & Plastics
Trade Name Durafoam™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Monmouth Rubber & Plastics Durafoam™ P192HD EPDM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Note 1: The Durafoam™100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ¼ inch thick sheets. These test pieces were exposed for 120 hours to a cycle consisting of: 1. Light at 70°C for 8 hours 2. Dark at 50° C for 4 hours 3. Condensation Cooling for 15 minutesInformation provided by Monmouth Rubber & Plastics Corp.
Physical Properties Metric English Comments
Linear Mold Shrinkage <= 0.017 cm/cm
<= 0.017 in/in
Descriptive Properties Value Comments
Color Grey