Monmouth Rubber & Plastics Durafoam™ C210FR Neoprene/EPDM/Polymeric Blend

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Monmouth Rubber & Plastics
Trade Name Durafoam™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Monmouth Rubber & Plastics Durafoam™ C210FR Neoprene/EPDM/Polymeric Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: High Heat Resistance Low Compression SetDimensionally Stable (Very Low Shrinkage) Unique Soft, Supple, Real Rubber Feel Very Fine Cell Structure High Coefficient of Friction for anti-skid applications such as mouse pads Bonds well to most pressure sensitive adhesives including economy rubber based products Available standard in gray and light tan Available on special order in custom colorsInformation provided by Monmouth Rubber & Plastics Corp.
Physical Properties Metric English Comments
Density 0.0881 g/cc
0.00318 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore OO 40
40
Elongation at Break 305 %
305 %
Compression Set 20 %
20 %
Suffix B, 25% max; ASTM D1056
Descriptive Properties Value Comments
Chemical Stability Acid, Dilute
Good
Aliphatic Hydrocarbons
Excellent
Animal, Vegetable Oils
Excellent
Aromatic Hydrocarbons
Excellent
Chlorinated Solvents
Fair to Good
Gasoline, Fuel Oil
Excellent
Lubricating Oils
Excellent
Natural Gas
Excellent
Oxidation Resistance
Excellent
Oxygenated Solvents
Fair to Good
Petroleum, Crude
Excellent
Sodium Hydroxides
Good
Water Swell Resistance
Excellent
Color Off-White