Momentive Performance Materials TSE399 One Component RTV Adhesive Sealant/Coating, Clear/White/Black

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials TSE399 One Component RTV Adhesive Sealant/Coating, Clear/White/Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TSE392, TSE397 and TSE399 adhesive sealants/coatings are one component RTV’s that cure quickly by reacting with atmospheric moisture forming a soft dielectric silicone rubber. These materials incorporate a newly developed crosslinking chemistry and are non-corrosive to metallic substrates. They are particularly well suited for electrical/electronic applications.This series of products differ in consistency, TSE392 is a thixotropic paste, TSE397 is semi-flowable, and TSE399 is flowable. When cured, they retain their elastomeric properties throughout the operating range of temperature from -55C to 200°C (-67F to 392F).Product Features: Meets the corrosion resistant requirements of MIL-A-46146AFast cure at ambient temperaturesOdor, slight alcoholOutstanding adhesion, including most plasticsOutstanding electrical propertiesResistant to heat, cold, moisture, UV, ozone and chemicalsProduct Benefits: One component, no mixing or de-airing requiredSoft consistency provides protection against mechanical and thermal shockExcellent electrical insulationProtects against moistureVarying viscosities allow thorough coating around complex assemblies (TSE399) and thicker coatings where required i.e., high voltage components (TSE392 & TSE397).Convenient packaging/dispensing tubes or cartridges.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
Viscosity 2500 cP

@Temperature 23.0 °C
2500 cP

@Temperature 73.4 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Tensile Strength, Ultimate 1.27 MPa
185 psi
Elongation at Break 140 %
140 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
Dielectric Constant 2.9

@Frequency 60 Hz
2.9

@Frequency 60 Hz
Dielectric Strength 20.0 kV/mm
508 kV/in
Dissipation Factor 0.0050

@Frequency 60 Hz
0.0050

@Frequency 60 Hz
Processing Properties Metric English Comments
Cure Time 10.0 min
0.167 hour
Tack free
Descriptive Properties Value Comments
Color Clear/White/Black
Consistency Flowable