Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials Silplusâ„¢ 80 EX Heat Cured Rubber - Extrusion

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name Silplus™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials Silplusâ„¢ 80 EX Heat Cured Rubber - Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance standards.Silplus 80 EX is a peroxide curable, extrusion grade, silicone elastomer.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
Tensile Strength 10.0 MPa
1450 psi
Elongation at Break 440 %
440 %
Tear Strength 28.0 kN/m
160 pli
Die B
Optical Properties Metric English Comments
Transmission, Visible 20 %
20 %
translucent; thickness unknown
Compliance Properties Metric English Comments
FDA Yes
Yes
FDA Indirect food contact - Rubber articles intended for repeated use - FDA Reg 21CFR177.2600
USP Class VI Yes
Yes
USP Class VI methods: Intramuscular implantation, intracutaneous injection, & systematic injection
Descriptive Properties Value Comments
Appearance Translucent
BfR product is compositionally compliant
Recommendation XV Silicones; post cured (4h/200°C)
ISO10993 yes
7 ISO 10993 tests applicable to "wet" chemicals
Water Regulations compliant
WRAS