Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials LVG342A Low Volatile Silicone Adhesive Component, White

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials LVG342A Low Volatile Silicone Adhesive Component, White.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LVG342 low volatile silicone adhesive is a two component, thixotropic silicone adhesive that cures very quickly at elevated temperatures to a durable elastomer. LV342 was specifically developed for applications that are sensitive to volatile siloxane species. For many applications, LVG342 is able to provide a very low level of volatility and out-gassing without the need for an extended post-cure bake cycle.Key Performance Properties: Very low controlled out-gassing and silicone volatilesVery fast cure at elevated temperaturesPrimerless adhesion to many substratesOutstanding compression set and CSR propertiesExcellent dielectric propertiesIdeal consistency for robotic dispensingExtended operating temperature performanceApplications: LVG342 low volatile silicone adhesive may be suitable for use in applications where the end-use application requires the high performance characteristics of a silicone, but is potentially functionally sensitive to low molecular weight, volatile siloxane species which may be released, via out-gassing, from a standard silicone polymer.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Processing Properties Metric English Comments
Cure Time 10.00000 min

@Temperature 175 °C
0.1666667 hour

@Temperature 347 °F
15.0 min

@Temperature 150 °C
0.250 hour

@Temperature 302 °F
20.0 min

@Temperature 125 °C
0.333 hour

@Temperature 257 °F
Descriptive Properties Value Comments
Application rate 150 g/min
Color White
Mix Ratio 10
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved