Material Notes:
Applications: Lead-free NVIS blue filter glass for Nichia White LED sources.Information provided by Mo-Sci Corporation.
Physical Properties Metric English Comments
Density 3.40 g/cc
0.123 lb/in³
Thickness 1000 microns
39.4 mil
Thermal Properties Metric English Comments
CTE, linear 12.0 µm/m-°C
6.67 µin/in-°F
Transformation Temperature, Tg 403 °C
757 °F
Softening Point 435 °C
815 °F
Dilatometric
Optical Properties Metric English Comments
Refractive Index 1.59
1.59
Transmission, Visible 30.4 %
30.4 %
Photopic, Source NSCW100
31.3 %
31.3 %
Photopic, Source NSCW455
UV Transmittance 0.070 %

@Wavelength 380 nm
0.070 %

@Wavelength 380 nm
0.070 %

@Wavelength 580 nm
0.070 %

@Wavelength 580 nm
0.60 %

@Wavelength 520 nm
0.60 %

@Wavelength 520 nm
0.60 %

@Wavelength 500 nm
0.60 %

@Wavelength 500 nm
0.61 %

@Wavelength 510 nm
0.61 %

@Wavelength 510 nm
Descriptive Properties Value Comments
Chromaticity, CIE 1976 0.15
u', Source NSCW455
0.16
u', Source NSCW100
0.22
v', Source NSCW100
0.23
v', Source NSCW455
NVIS Radiance 4.4E-12
NR(b), MIL-STD-3009@0.1 fL Luminance, Source NSCW455
4.5E-12
NR(b), MIL-STD-3009@0.1 fL Luminance,, Source NSCW100
5.7E-11
NR(a), MIL-STD-3009@0.1 fL Luminance, Source NSCW455
5.9E-11
NR(a), MIL-STD-3009@0.1 fL Luminance, Source NSCW100
Tolerance Radius 0.01
r', Source NSCW007
0.01
r', Source NSCW100
0.01
r', Source NSCW455