Möller Medical NanoSkin Magic 101 L NanoCoating

Category Ceramic , Glass , Glass Ceramic , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Moeller Medical (Möller Medical)
Trade Name NanoSkin Magic
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Möller Medical NanoSkin Magic 101 L NanoCoating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conducting coating with very good chemical resistance, biocompatible, becoming hydrophilic after water contactInformation provided by Möller Medical, Member of CENTROTEC Group
Physical Properties Metric English Comments
Thickness 3.00 - 10.0 microns
0.118 - 0.394 mil
Mechanical Properties Metric English Comments
Taber Abrasion, mg/1000 Cycles 68
68
CS17 friction disc with 500g load; DIN 53754
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Processing Properties Metric English Comments
Processing Temperature 300 - 380 °C
572 - 716 °F
Hardening Temperature
Descriptive Properties Value Comments
Applicable Substrate Aluminum
Brass
with restrictions
Copper
Glass
with restrictions
Stainless Steel
Tubes int. dia. 0.1-10 mm
with restrictions
Biocompatibility Biocompatible
One-parametric cytotoxicity test
Contact Angle to Water [deg] 101
Cupping Test [mm] 6
DIN EN ISO 1520
Non-Applicable Substrate ABS
Nylon
PMMA
Polycarbonate
Pendulum Dampening Test [sec] 140-160
DIN EN ISO 1522