Material Notes:
EXCEREX™ is an innovative processing improvement agent created with metallocene catalysis technology. EXCEREX™ gains in a number of ares simultaneously, including faster processing speeds, lower resin temperatures, reduced scorching, and reduced changeover times.Information provided by Mitsui Chemicals
Physical Properties Metric English Comments
Density 0.912 g/cc
0.0329 lb/in³
Molecular Weight 2900 g/mol
2900 g/mol
Thermal Properties Metric English Comments
Melting Point 102 °C
216 °F
Softening Point 105 °C
221 °F