Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Amorphous  (discontinued **)

Category Polymer , Thermoplastic , Polyimide, Thermoplastic
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Amorphous  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to its semicrystalline state. In addition, it displays low outgassing, superior radiation resistance and excellent chemical resistance properties.Applications: Components for automotive and aircraft enginesTransmissionFarming, off-road and construction equipmentIndustrial machineryElectric motors, pumps and compressorsBusiness machines such as laser pointers and high speed copy machinesElectronic and semiconductor transport mediaAnalytical and medical equipmentConveyors and textile equipmentInformation provided by Mitsui.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Water Absorption 0.24 %
0.24 %
24 hours; ASTM D570
Moisture Absorption at Equilibrium 0.10 %
0.10 %
24 hours, 23°C, 60% RH
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 100
100
ASTM D785
Hardness, Rockwell R 123
123
ASTM D785
Tensile Strength at Break 249.1 MPa
36130 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 356 MPa
51600 psi
ASTM D790
Flexural Modulus 20.4 GPa
2960 ksi
ASTM D790
Izod Impact, Notched 1.18 J/cm
2.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 6.00 µm/m-°C

@Temperature 23.0 °C
3.33 µin/in-°F

@Temperature 73.4 °F
MD; ASTM D696
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 °C
26.1 µin/in-°F

@Temperature 73.4 °F
ASTM D696
Thermal Conductivity 0.4883 W/m-K
3.383 BTU-in/hr-ft²-°F
Melting Point 388 °C
730 °F
Maximum Service Temperature, Air 240 °C
464 °F
Heat distortion temperature, load unknown; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1000 - 10000 ohm
1000 - 10000 ohm
ASTM D257
Processing Properties Metric English Comments
Processing Temperature 390 - 420 °C
734 - 788 °F
Injection molding, extrusion