Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Minelco MicaFil Vermiculite

Category Ceramic , Oxide , Magnesium Oxide , Silicon Oxide
Manufacturer Minelco Inc.
Trade Name MicaFil
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Minelco MicaFil Vermiculite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vermiculite is the geological name given to a group of hydrated laminar minerals which are aluminum iron magnesium silicates resembling mica in appearance.Vermiculite is a safe inert material, light in color.When heated it expands up to 30 times its original volume converting dense flakes into lightweight, porous granules containing innumerable minute air layers.Exfoliated vermiculite is light and clean to handle, has a high insulation value, acoustic insulating properties and will absorb and hold a range of liquids. The granules are non-combustible and are insoluble in water and organic solvents. Applications: Heat and Acoustic insulation, floor and roof screeds, flue linings, passive fire protection, cements, construction boards and panels.
Descriptive Properties Value Comments
Appearance Expanded granules
Users viewing this material also viewed the following: