Minelco Chilcon Low grade FeSi

Category Ceramic , Metal , Intermetallic
Manufacturer Minelco Inc.
Trade Name Chilcon
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Minelco Chilcon Low grade FeSi.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hard, wear resistant. Applications: Heavy aggregates, hard wearing floors
Physical Properties Metric English Comments
Particle Size 500 - 5000 µm
500 - 5000 µm
Component Elements Properties Metric English Comments
Iron, Fe 78 - 80 %
78 - 80 %
Silicon, Si 15 %
15 %
Descriptive Properties Value Comments
Appearance Silvery granular product