Minelco 44 Sarca Chamottes

Category Ceramic , Clay , Oxide , Aluminum Oxide
Manufacturer Minelco Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Minelco 44 Sarca Chamottes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extremely consistent. Applications: Manufacture of mid alumina fired and monolithic refractory and foundry products
Component Elements Properties Metric English Comments
Al2O3 >= 44 %
>= 44 %
Fe2O3 <= 1.1 %
<= 1.1 %
TiO2 2.0 %
2.0 %
Descriptive Properties Value Comments
Appearance Grey Pellets