Mid-Mountain Materials SILTEX® 1800 Amorphous Silica Industrial Textile

Category Ceramic , Glass , Glass Fiber , Oxide , Silicon Oxide
Manufacturer Mid-Mountain Materials
Trade Name SILTEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mid-Mountain Materials SILTEX® 1800 Amorphous Silica Industrial Textile.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SILTEX® 1800 is a family of high performance textiles comprised of high purity, high strength amorphous silica fibers. SILTEX® 1800 Industrial Textiles demonstrate excellent thermal stability, have insulating values up to 1800ºF (980ºC), and are designed for use where severe temperature conditions exist.Information provided by Mid-Mountain Materials
Thermal Properties Metric English Comments
Melting Point 1260 °C
2300 °F
Maximum Service Temperature, Air 982 °C
1800 °F
Continuous
1260 °C
2300 °F
Short term
Component Elements Properties Metric English Comments
SiO2 96 %
96 %
Descriptive Properties Value Comments
Abrasion Resistance Poor
Acid Resistance Good
Alkali Resistance Poor
Certification MIL-I-24244
May be manufactured for conformance
Color White or Tan
Solvent Resistance Excellent
Sunlight and Aging Resistance Excellent