Mid-Mountain Materials CERMEX® PR1000-P Premium Grade Thermal Insulation Paper

Category Ceramic , Glass , Glass Fiber , Other Engineering Material , Composite Fibers
Manufacturer Mid-Mountain Materials
Trade Name CERMEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mid-Mountain Materials CERMEX® PR1000-P Premium Grade Thermal Insulation Paper.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material: Non-respirable E-glass fibers Construction: Felted paper, organic binderInformation provided by Mid-Mountain Materials
Physical Properties Metric English Comments
Density 0.139 g/cc

@Thickness 3.17 mm
0.00503 lb/in³

@Thickness 0.125 in
0.184 g/cc

@Thickness 0.762 mm
0.00666 lb/in³

@Thickness 0.0300 in
0.184 g/cc

@Thickness 1.52 mm
0.00666 lb/in³

@Thickness 0.0600 in
0.192 g/cc

@Thickness 0.381 mm
0.00694 lb/in³

@Thickness 0.0150 in
Loss On Ignition 5.0 - 7.0 %
5.0 - 7.0 %
Thickness 380 microns
15.0 mil
760 microns
29.9 mil
1587 microns
62.48 mil
3175 microns
125.0 mil
Thermal Properties Metric English Comments
Thermal Conductivity 0.0300 W/m-K

@Temperature 24.0 °C
0.208 BTU-in/hr-ft²-°F

@Temperature 75.2 °F
0.0400 W/m-K

@Temperature 120 °C
0.278 BTU-in/hr-ft²-°F

@Temperature 248 °F
0.0600 W/m-K

@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.0800 W/m-K

@Temperature 400 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 752 °F
0.150 W/m-K

@Temperature 650 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Melting Point >= 1100 °C
>= 2010 °F
Fiber Only
Maximum Service Temperature, Air 538 °C
1000 °F
Continuous
649 °C
1200 °F
Intermittent
Descriptive Properties Value Comments
Color White
Shot Content (%) None
Tensile Strength (lbs/in) 11
1/64", Cross Direction
12
1/64", Machine Direction
20
1/32", Cross Direction
21
1/32", Machine Direction
44
1/16", Machine Direction
45
1/8", Machine Direction
47
1/16", Cross Direction
50
1/8", Cross Direction
Width (in) 51