Micropol Microcoat DG/EVA/214A Microground modified EVA copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Micropol Limited
Trade Name Microcoat
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Micropol Microcoat DG/EVA/214A Microground modified EVA copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specially developed for high specification coating where metal/coating adhesion is of primary importance. Typically used on large flat surfaces, and when toughness, elasticity and excellent barrier properties are needed. Information provided by Micropol Limited
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Particle Size 180 - 350 µm
180 - 350 µm
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238 E
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.0 MPa
2320 psi
ASTM D638
Tensile Strength, Yield 3.50 MPa
508 psi
ASTM D638
Elongation at Break 600 %
600 %