Micropol DD Polyethylene powders for cleaning products

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Micropol Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Micropol DD Polyethylene powders for cleaning products.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Micropol Limited
Physical Properties Metric English Comments
Bulk Density 0.300 g/cc
0.0108 lb/in³
ASTM D1895
Density 0.916 g/cc
0.0331 lb/in³
ASTM D792
Particle Size <= 350 µm
<= 350 µm
ASTM D1921