Michelman® SofTak® 126 Non-skid coating

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name SofTak®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® SofTak® 126 Non-skid coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Non-skid coating.Usage: SofTak® 126 is a gluable nonskid coating with the added benefit of good scuff and water resistance, oil resistance and a "leather like" feel. This product is effective for slip or tier sheets as well as decorative packaging.Application Data: SofTak® 126 does not require specific drying parameters. SofTak® 126 can be applied by rod coater.Softak® is typically used for: Slip or tier sheets to prevent slipping of palletized loads, boxes and furniture; Coated paper used as temporary flooring where skid resistance is critical; Protective floor mats for highly-polished surfaces during moving phase; and Jewelry and perfume packagingFood Contact Information when manufactured in Belgium: FDA: 175.105: Components of adhesives.176.180: Components of paper and paperboard in contact with dry foods.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.02 - 1.04 g/cc
1.02 - 1.04 g/cc
pH 7.2 - 9.2
7.2 - 9.2
Brookfield Viscosity 100 - 700 cP
100 - 700 cP
Spindle # 3, rpm 60
Descriptive Properties Value Comments
Appearance Milky white liquid
Solids Type Polymer