Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Michelman® RustBan® 250 Corrosion inhibitor coating

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® RustBan® 250 Corrosion inhibitor coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Corrosion inhibitor coatingUsage: RustBan® 250 is a Vapor Corrosion Inhibitor for the protection of ferrous and nonferrous metals. This product can be applied to corrugated, solid fiber and other forms of paperboard packaging. RustBan® 250 is both hot melt and cold set gluable.Application Data: RustBan® 250 can be applied in-line or off-line by blade or rod coater.RustBan® has a wide range of applications: Auto/Heavy Equipment; Steel Mills; Consumer Packaging; Electronics; and MilitaryInformation provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.15 - 1.17 g/cc
1.15 - 1.17 g/cc
pH 10 - 11
10 - 11
Brookfield Viscosity <= 50 cP
<= 50 cP
Spindle # 1, rpm 60
Viscosity Measurement 15 - 19
15 - 19
[sec], EZ cup, Cup # 2
Descriptive Properties Value Comments
Appearance Yellow, thin liquid
Solids Type Corrosion Inhibitor