Michelman® Michem® Shield 422 Anionic dispersion of polyethylene wax

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Michelman®
Trade Name Michem® Shield
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Shield 422 Anionic dispersion of polyethylene wax.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Anionic dispersion of polyethylene waxUsage: Michem® Shield 422 provides superior rub resistance in graphic arts applications.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.970 - 0.990 g/cc
0.970 - 0.990 g/cc
Volatiles 49.5 - 50.5 %
49.5 - 50.5 %
pH 4.0 - 10
4.0 - 10
Brookfield Viscosity <= 1000 cP
<= 1000 cP
Spindle # 3, rpm 60
Descriptive Properties Value Comments
Appearance White liquid
Emulsifier Charge Anionic
Solids Type Polyethylene