Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Michelman® Michem® Prime 5931 Modified ethylene acrylic acid dispersion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Ethylene Acrylic Acid
Manufacturer Michelman®
Trade Name Michem® Prime
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Prime 5931 Modified ethylene acrylic acid dispersion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Modified ethylene acrylic acid dispersionUsage: Michem®Prime 5931 is a modified ethylene acrylic acid dispersion which provides improved adhesion to polyolefin substrates. It also exhibits excellent adhesion to paper, metallic and polymeric substrates as well as glass and polyester scrim. It can serve as a tie coat or primer and increases printability on metallic and polymeric substrates. It can be used as a heat sealable coating on most polymeric films, paper and foil. Patents Pending.Application Data: Michem®Prime 5931 can be applied by flexographic or rotogravure coating methods. A typical application rate of 1-2 gsm dry coating weight is recommended for most heat seal applications. As a tie coat or print primer application rates of 0.2 to 0.5gsm are usually sufficient.Food Contact Information when manufactured in the USA and Belgium: FDA:175.105: Components of adhesives(Restricted)175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted) 176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)176.180: Components of paper and paperboard in contact with dry foods. (Restricted)Food Contact Information when manufactured in Singapore: FDA:175.105: Components of adhesives(Restricted) 175.300: Resinous and polymeric components of coatings. (Restricted) 175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted) 176.180: Components of paper and paperboard in contact with dry foods.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.990 - 1.01 g/cc
0.990 - 1.01 g/cc
Volatiles 71 - 72.5 %
71 - 72.5 %
pH >= 7.0
>= 7.0
Recommended pH of system
8.0 - 10
8.0 - 10
Brookfield Viscosity <= 100 cP
<= 100 cP
Spindle # 3, rpm 60
Descriptive Properties Value Comments
Appearance White translucent liquid
Emulsifier Charge Ammoniated dispersion
Solids Type Proprietary