Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Michelman® Michem® Guard 349 Nonionic, polyethylene dispersion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Michelman®
Trade Name Michem® Guard
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Guard 349 Nonionic, polyethylene dispersion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nonionic, polyethylene dispersionUsage: Michem® Guard 349 is designed to impart rub resistance, block resistance and matting properties to aqueous paints, coatings and inks.Typical uses include: Inks and OPVs; Exterior wood and wood composites and Interior furniture and flooringFood Contact Information when manufactured in Belgium:FDA:175.300: Resinous and polymeric components of coatings. (Restricted) 176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted) 176.180: Components of paper and paperboard in contact with dry foods. (Restricted)Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.960 - 0.980 g/cc
0.960 - 0.980 g/cc
Volatiles 49.5 - 50.5 %
49.5 - 50.5 %
pH >= 7.0
>= 7.0
Recommended pH of system
6.5 - 8.5
6.5 - 8.5
Brookfield Viscosity 500 - 1000 cP
500 - 1000 cP
Spindle # 3, rpm 60
Descriptive Properties Value Comments
Appearance White liquid
Emulsifier Charge Nonionic
Solids Type Polyethylene
Users viewing this material also viewed the following: