Material Notes:
Description: Water based emulsion of montan based ester waxUsage: Michem® Emulsion 61222 is a bleached montan wax emulsion providing excellent slip and anti-blocking properties.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foamInformation provided by Michelman®
Physical Properties Metric English Comments
Volatiles 77.5 - 78.5 %
77.5 - 78.5 %
Descriptive Properties Value Comments
Appearance White, creamy liquid
Emulsifier Charge Nonionic
Solids Type Montan Based Ester wax